1 |
Heating glass |
1. Integral factor
light transmission ,Ò – ≥ 85%
2. integral factor
of mirror reflection, R – (1.5 – 2.0)%
3. Surface resistance of transparent current-conductive coating , within (8 - 30) Ohm/sq.
4. Surface resistance of current-conducting buses, within 0.05 –
0.1 Ohm/sq.
5. mechanical strength of coatings
group 0 under OSTÒ3-1901-84
6. Immunity to ambient exposures
– under GOST 20.57.406-81 |
diagonal – up to 21"
thickness – 2.0, 3.0, 4.0, 5.0, 6.0 mm and over
|
|
2 |
Heating glass for LC matrixes
|
1. Integral factor of light transmission,Ò – ≥ 85%
2.Integral factor of mirror reflection, R – , upon requirement
3. Surface resistance of transparent current-conducting
coating, within (8 –
30) Ohm/sq.
4. Surface resistance of current-conducting buses within 0.05- 0.10 Ohm/sq.
5. Mechanical strength of coatings – group 0 under OST3-1901-84
6 Immunity to outside exposure – under GOST 20.57.406-81 |
diagonal – up to 12"
thickness – 0.7, 1.1mm |